Investigation of dynamic micromechanical properties of biodegradable elastic material by continuous stiffness measurement analysis
(Sage Publications Ltd, 2023)Micromechanical properties of polymeric materials play a critical role in various biological applications in terms of their biocompatibility and mechanical durability. Apart from material properties such as modulus and ...