Monitoring the gelation of polyacrylamide-sodium alginate composite by fluorescence technique
(Taylor & Francis Ltd, 2012)
Polyacrylamide (PAAm)-sodium alginate (SA) composite was prepared with different amounts of SA varying in the range between 0.06% and 2% (w/v). The PAAm-SA composite was characterized by the steady-state fluorescence ...
Critical Exponents of Gelation and Conductivity in Polyacrylamide Gels Doped by Multiwalled Carbon Nanotubes
(Taylor & Francis Ltd, 2010)
Polyacrylamide (PAM) doped by multiwalled carbon nanotube (MWNT) gels were prepared with different amounts of MWNTs varying in the range between 0.1 and 15 wt%. The PAM-MWNT composite gels were characterized by the steady ...
Phase Transitions in Pure and Hybrid Hydrogels: A Fluorescence Study
(Wiley, 2009)
Recent observations on phase transitions around the critical point showed that the critical exponents differed drastically from percolation results and classical results for pure hydrogel systems depending on monomer ...