The Effect of Film Thickness and Tio2 Content on Film Formation From Ps/Tio2 Nanocomposites Prepared by Dip-Coating Method

dc.contributor.author Sunay, M. Selin
dc.contributor.author Pekcan, Mehmet Önder
dc.contributor.author Pekcan, Önder
dc.contributor.author Ugur, Saziye
dc.contributor.other Molecular Biology and Genetics
dc.date.accessioned 2019-06-27T08:04:26Z
dc.date.available 2019-06-27T08:04:26Z
dc.date.issued 2012
dc.department Fakülteler, Mühendislik ve Doğa Bilimleri Fakültesi, Biyoinformatik ve Genetik Bölümü en_US
dc.description.abstract Steady-state fluorescence (SSF) technique in conjunction with UV-visible (UVV) technique and atomic force microscope (AFM) was used for studying film formation from TiO2 covered nanosized polystyrene (PS) latex particles (320 nm). The effects of film thickness and TiO2 content on the film formation and structure properties of PS/TiO2 composites were studied. For this purpose two different sets of PS films with thicknesses of 5 and 20 mu m were prepared from pyrene-(P-) labeled PS particles and covered with various layers of TiO2 using dip-coating method. These films were then annealed at elevated temperatures above glass transition temperature (T-g) of PS in the range of 100-280 degrees C. Fluorescence emission intensity I-p from P and transmitted light intensity I-tr were measured after each annealing step to monitor the stages of film formation. The results showed that film formation from PS latexes occurs on the top surface of PS/TiO2 composites and thus developed independent of TiO2 content for both film sets. But the surface morphology of the films was found to vary with both TiO2 content and film thickness. After removal of PS thin films provide a quite ordered porous structure while thick films showed nonporous structure. en_US]
dc.identifier.citationcount 3
dc.identifier.doi 10.1155/2012/524343 en_US
dc.identifier.issn 1687-4110 en_US
dc.identifier.issn 1687-4110
dc.identifier.scopus 2-s2.0-84862298267 en_US
dc.identifier.uri https://hdl.handle.net/20.500.12469/939
dc.identifier.uri https://doi.org/10.1155/2012/524343
dc.identifier.wos WOS:000305021700001 en_US
dc.institutionauthor Pekcan, Önder en_US
dc.language.iso en en_US
dc.publisher Hindawi Publishing Corporation en_US
dc.relation.journal Journal of Nanomaterials en_US
dc.relation.publicationcategory Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı en_US
dc.rights info:eu-repo/semantics/openAccess en_US
dc.scopus.citedbyCount 3
dc.title The Effect of Film Thickness and Tio2 Content on Film Formation From Ps/Tio2 Nanocomposites Prepared by Dip-Coating Method en_US
dc.type Article en_US
dc.wos.citedbyCount 3
dspace.entity.type Publication
relation.isAuthorOfPublication e5459272-ce6e-44cf-a186-293850946f24
relation.isAuthorOfPublication.latestForDiscovery e5459272-ce6e-44cf-a186-293850946f24
relation.isOrgUnitOfPublication 71ce8622-7449-4a6a-8fad-44d881416546
relation.isOrgUnitOfPublication.latestForDiscovery 71ce8622-7449-4a6a-8fad-44d881416546

Files

Original bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
The effect of film thickness and TiO2 content on film formation from PS TiO2 nanocomposites prepared by dip-coating method.pdf
Size:
6.12 MB
Format:
Adobe Portable Document Format
Description: